Rubber-Based Hot Melt Adhesive Label Stock — Cold Chain
Two adhesives, two different jobs
Acrylic adhesive is the default because it is clean, ages well and survives sunlight. Rubber-based hot melt does one thing acrylic cannot: it grips on contact. Where a label is applied to a frozen carton, a dusty fibreboard box or a surface with condensation on it, the acrylic needs time and pressure to wet out — and it never gets either on a packing line. Hot melt with high initial tack holds immediately, which is why cold chain and recycled board are its natural territory.

Specifications
| Adhesive | Rubber-based hot melt, high initial tack |
| Face stock | Direct thermal, semi-gloss, woodfree, BOPP |
| Liner | Glassine 40–58 gsm, white / yellow |
| Max width | 1,530 mm |
| Roll length | 1,000–6,000 m |
| Service range | Freezer grade versions for −20 °C and below |
Where hot melt wins and where it does not
- Wins: frozen and chilled cartons, recycled fibreboard with a rough surface, application at low temperature, short dwell time on a fast line.
- Wins: single-use shipping labels where the label never needs to come off again.
- Loses: outdoor and UV-exposed labels — rubber degrades and the adhesive yellows.
- Loses: removable or repositionable applications — hot melt grips permanently by design.
What to state when ordering
The application temperature, the surface (board, film, metal, glass), how long the label has before it must hold, and whether it is ever removed. A freezer label applied at −18 °C and a warehouse label applied at 25 °C are different products even when the face stock looks identical.
Buyers also search for this product as
etykiety z klejem kauczukowym · etykiety z klejem akrylowym · rubber based adhesive labels · hot melt adhesive label stock · freezer grade label stock · cold chain labels · etiquetas con adhesivo hot melt · Klebstoff Hotmelt Etiketten
Ordering
Send the face stock, width, roll length, liner colour and the application temperature. If the label goes onto a frozen product, say whether it is applied before or after freezing — that single detail changes the adhesive grade.